Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate

Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate

Titanium porous metal sintered plate is a type of material made from pure titanium powder. Sintered titanium plate has a porous structure with a high surface area and high porosity.
Invia la tua richiesta
Chatta adesso
Descrizione

 

Products Description Tel:0917-3664600

Titanium porous metal sintered plates are made from titanium powder through the process of cold pressing, sintering, and hot pressing. This manufacturing technique produces a product that is highly porous with a range of pore sizes and interconnected channels to maximize filtration efficiency.

Product features:

Some key features of titanium porous metal sintered plates include:

High porosity: The porosity of titanium porous metal sintered sheets ranges from 30% to 50%, which enables effective filtration while allowing for high flow rates.
Chemical resistance: Titanium is known for its excellent corrosion resistance in a broad range of acidic and alkaline environments, which makes it suitable for use in a wide range of industrial applications.
High temperature resistance: Titanium sintered plates have a high melting point of 1668°C, allowing these plates to perform well in high-temperature applications.
Durability: Titanium sintered sheets are durable and resistant to wear, which makes them suitable for applications where the filtration material may experience high stress or be subjected to frequent cleaning cycles.
Customizability: Titanium porous metal sintered plates can be customized to meet specific filtration requirements, including pore size, thickness, and shape.

titanium Sintered Porous Plate price
Specification Tel:0917-3664600
Grade Gr1 pure titanium 
Size 0.5mm to 10mm; 1μm to 100μm; 
Porosity 20% to 60%
Melting point 1668°C
Factory Tour Tel:0917-3664600
Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate
Porous titanium disc for sale
Titanium sintered sheet Titanium sintered filter
Common use titanium sintered porous plate Tel:0917-3664600

The grade of titanium used to produce the porous metal sintered plate is typically Grade 1, which is a commercially pure form of titanium that has excellent corrosion resistance and good mechanical properties.

The product parameters of titanium porous metal sintered plate can vary depending on the application. Some common parameters include thickness, pore size, and porosity. The thickness can range from 0.5mm to 10mm, while the pore size can range from 1μm to 100μm. The porosity, or the ratio of the void volume to the total volume, can range from 20% to 60%.

Applications of titanium sintered porous sheet Tel:0917-3664600

The applications of titanium porous metal sintered plate are varied and can include filtration, gas and liquid diffusion, catalyst support, and electrode materials in electrochemical systems. Due to its high surface area, the material is often used in biomedical applications such as bone implants and tissue engineering scaffolds. It is also utilized in the aerospace industry for applications such as heat exchangers and acoustic damping materials. Overall, Sintered titanium metal sheet offers excellent mechanical, thermal, and chemical stability, making it a versatile material for a range of applications.

Packing And Shipping Tel:0917-3664600

details4-5.jpg

details4-6.jpg

Other related sintered titanium metal sheet and porous titanium disc

buy porous titanium plate

Porous Titanium Sintered Plates

Etichetta sexy: sintered porous plate 1mm thickness titanium porous metal sintered plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China

Invia la tua richiesta

(0/10)

clearall